This is a SE SEM image of the device die. The source bond wire (left) was fused open. The gate bond wire (right) was intact.
This is the source bond pad. This material (arrow) is fused gold-copper-silica-silicon.
The source bond wire is fused open suggesting excessive source current caused the failure.
Check out SEM Lab, Inc. to learn more.